Physical Properties Metric English Comments
Density 9.3074 g/cc
0.33625 lb/in³
CMW® D50F Silver Nickel Alloy
CMW® D50F can be fabricated into wire, rod and strip; however, the headability of CMW® D50F is limited to a narrow range. It is used for main contacts in circuit breakers and switching devices whe..