Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.13 g/cc | 0.258 lb/in³ | |
MarkeTech BGO (Bismuth Germanate, Bi4Ge3O12) Scintillator Crystal Bismuth germanate is intrinsic scintillation material with high absorption power. Due to its high effective atomic number and high density, BGO is a very efficient gamma absorber with high photo eff.. |
|||
Density | 7.15 g/cc | 0.258 lb/in³ | |
Resistalloy International Fecralloy™ Electrical Resistance Steel Yttrium addition does not appear in nominal composition. Ferritic stainless steel with aluminum. Available as wire, bar, tube, and strip. Used mainly for electrical elements in both industrial and.. |