Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 6.80 - 7.00 g/cc | 0.246 - 0.253 lb/in³ | |
Pacific Sintered Materials F-241-S1 Iron Soft Magnetic Powdered Metal Applications: DC magnetic applications such as pole pieces, cores, armatures, generator rotors and stator cores.Equivalent ASTM Specification: B310-70, TYPE III, CLASS AAll information provided by P.. |
|||
Density | 6.80 - 7.00 g/cc | 0.246 - 0.253 lb/in³ | |
PSM Industries Pacific Sintered Metals Iron F-241-S1 Powdered Metal DC magnetic applications such as pole pieces, cores, armatures, generator rotors and stator cores Equivalent ASTM Spec: B310-70, Type III, Class AInformation Provided by Pacific Sintered Metals, a .. |