Polymer Property : Density = 0.231 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 6.40 - 6.80 g/cc
0.231 - 0.246 lb/in³
Pacific Sintered Materials BT-121-R Bronze Powdered Metal
Applications: Structural and bearing bronze.Equivalent MPIF Specification: CT-1000-K23All information provided by Pacific Sintered Metals.
Density 6.40 - 6.80 g/cc
0.231 - 0.246 lb/in³
Pacific Sintered Materials SS-316-RD 316L Stainless Steel Powdered Metal
Non-magnetic, non-hardenable stainless steel for mechanical and instrumental components requiring corrosion resistance.Equivalent MPIF Specification: SS-316-40All information provided by Pacific Sin..
Density 6.40 - 6.80 g/cc
0.231 - 0.246 lb/in³
Pacific Sintered Materials SS-316-RH 316L Stainless Steel Powdered Metal
Non-magnetic, non-hardenable stainless steel for mechanical and instrumental components requiring corrosion resistance.All information provided by Pacific Sintered Metals.
Density 6.40 - 6.80 g/cc
0.231 - 0.246 lb/in³
Pacific Sintered Materials SS-410-R 410 Stainless Steel Powdered Metal
Magnetic stainless steel with high strength and good wearing properties.Equivalent MPIF Specification: SS-410-95All information provided by Pacific Sintered Metals.
Density 6.40 - 6.80 g/cc
0.231 - 0.246 lb/in³
PSM Industries Pacific Sintered Metals 316L Stainless Steel SS-316-RD Powdered Metal
Non-magnetic, non-hardenable stainless steel for mechanical and instrumental components requiring corrosion resistance. Equivalent MPIF Specification: SS-316-40Information Provided by Pacific Sinte..
Density 6.40 - 6.80 g/cc
0.231 - 0.246 lb/in³
PSM Industries Pacific Sintered Metals 316L Stainless Steel SS-316-RH Powdered Metal
Non-magnetic, non-hardenable stainless steel for mechanical and instrumental components requiring corrosion resistance.Information Provided by Pacific Sintered Metals, a division of PSM Industries
Density 6.40 - 6.80 g/cc
0.231 - 0.246 lb/in³
PSM Industries Pacific Sintered Metals 410 Stainless Steel SS-410-R Powdered Metal
Magnetic stainless steel with high strength and good wearing properties Equivalent MPIF Specification: SS-410-95Information Provided by Pacific Sintered Metals, a division of PSM Industries
Density 6.40 - 6.80 g/cc
0.231 - 0.246 lb/in³
PSM Industries Pacific Sintered Metals Bronze BT-121-R Powdered Metal
Structural and bearing bronze Equivalent MPIF Specification: CT-1000-K23Information Provided by Pacific Sintered Metals, a division of PSM Industries
Density 6.40 g/cc
0.231 lb/in³
China Tungsten NT3 Titanium Carbonitride Alloy
Titanium carbonitride base alloy , also called cermets, with of high hardness, good red hard-ness and wear resistance, medium toughness, high  corrosion resistance to acids and alkalis and hi-tempe..
Density 6.39 g/cc
0.231 lb/in³
Ametek P304L P/M Stainless Steel, Sintered from 6.25 g/cc Green Density
Powder apparent bulk density 2.7 g/cc; powder flow 30 sec/50g.Compacting properties measured on powders with 1% lithium stearite. Sintering was done in dissociated ammonia at 1121°C (2050°F) for ..