Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 6.32 g/cc
0.228 lb/in³
Indium Corp. Indalloy 51E Low Melting Gallium Alloy
Information Provided by Indium Corporation
Density 6.30 g/cc
0.228 lb/in³
China Tungsten NT5 Titanium Carbonitride Alloy
Titanium carbonitride base alloy , also called cermets, with of high hardness, good red hard-ness and wear resistance, medium toughness, high  corrosion resistance to acids and alkalis and hi-tempe..
Density 6.30 - 6.70 g/cc
0.228 - 0.242 lb/in³
China Tungsten ST1645 PM Antifriction Parts
Information provided by China Tungsten
Density >= 6.30 g/cc
>= 0.228 lb/in³
China Tungsten STG10-10 PM Structural Parts
Information provided by China Tungsten
Density 6.30 g/cc
0.228 lb/in³
CMW® D1058 Silver Graphite Contact Material
For electrical contacts, resistant to sliding wear.Information provided by CMW Inc.
Density 6.30 - 6.90 g/cc
0.228 - 0.249 lb/in³
China Tungsten ST2365 PM Antifriction Parts
Information provided by China Tungsten