Density 6.22 g/cc
0.225 lb/in³
Ferro CF 8463 Low-Temperature Sealing
VITREOUS Typical Powder Form: VSD, VWG Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific..