Polymer Property : Density = 0.186 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 5.15 g/cc
0.186 lb/in³
Ferro EG 2739 Thick Film Glass
Glass Type: Pb-Zn-B Typical Powder Form: MVG Typical Application: Resistor Overglaze Ferro produces standard and custom glass products that are used in thick film compositions including resistors, ..