Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 5.04 g/cc | 0.182 lb/in³ | |
Ferro CF 7586 Low-Temperature Sealing DEVITRIFYING Typical Powder Form: TF Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific t.. |
|||
Density | 5.03 g/cc | 0.182 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP MH0500C PP (Asia Pacific) LNP* Thermocomp* MH0500C is a compound based on Polypropylene resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Density | 5.04 g/cc | 0.182 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP MH0500C PP (Asia Pacific) LNP* Thermocomp* MH0500C is a compound based on Polypropylene resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Density | 5.03 g/cc | 0.182 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP MH0500C PP LNP* THERMOCOMP* MH0500C is a compound based on Polypropylene resin. Added feature of this material is: High Specific Gravity. |
|||
Density | 5.04 g/cc | 0.182 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP MH0500C PP LNP* THERMOCOMP* MH0500C is a compound based on Polypropylene resin. Added feature of this material is: High Specific Gravity. |