Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 4.86 g/cc | 0.176 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP WX02869H Polyester, TP LNP THERMOCOMP* WX02869H is a compound based on Polyester, TP resin containing High Specific Gravity. Added features of this material include: High Impact. |
|||
Density | 4.87 g/cc | 0.176 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP WX02869H Polyester, TP LNP THERMOCOMP* WX02869H is a compound based on Polyester, TP resin containing High Specific Gravity. Added features of this material include: High Impact. |