Physical Properties Metric English Comments
Density 3.98 g/cc
0.144 lb/in³
MarkeTech Sapphire (Aluminum Oxide - Al2O3) Single Crystal
Data provided by the supplier, MarkeTech International.Sapphire is grown by several methods: Boule form (Czochralski), in plate form, or as tubes, rods and plates. Boules are grown up to 8" diam..
Density 3.99 g/cc
0.144 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP AH0400A ABS
LNP* THERMOCOMP* AH0400A is a compound based on ABS resin. Added feature of this material is: High Specific Gravity.
Density 3.98 g/cc
0.144 lb/in³
Zircar Ceramics HC Sapphire (Single Crystal Aluminum Oxide) Hangar Clip
ZIRCAR hanger clips are comprised of sapphire (single crystal aluminum oxide) and are designed for use with hanger rod (HR-1). The single crystal structure of these clips prevents creep and deformat..
Density 3.98 g/cc
0.144 lb/in³
Goodfellow Ruby, Al2O3
Ruby exhibits identical properties to those of sapphire. Small amounts of impurities, especially chromium oxide, give ruby a red coloration. Useful optical range from 150 - 5500 nm.Information pro..
Density 3.98 g/cc
0.144 lb/in³
Anderman Ceramics EA999 Sintered Alumina, 99.9%
Densely sintered alumina is characterized by: high strength and hardness, temperature stability, electrical insulation, and high wear resistance and corrosion resistance even at high temperatures. ..
Density 3.98 g/cc
0.144 lb/in³
Mateck Sapphire (Al2O3)
Optical crystals
Density 3.98 g/cc
0.144 lb/in³
Mateck Sapphire Aluminium oxide Substrate, Al2O3
Substrate single crystals for superconductivity.