Polymer Property : Density = 0.130 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 2.60 - 3.60 g/cc
0.0939 - 0.130 lb/in³
Alliance BIF-11 Bonded (Composite) Magnetic Material
Density 2.60 - 3.60 g/cc
0.0939 - 0.130 lb/in³
Alliance BIF-17 Bonded (Composite) Magnetic Material
Density 2.60 - 3.60 g/cc
0.0939 - 0.130 lb/in³
Alliance BIF-19 Bonded (Composite) Magnetic Material
Density 2.60 - 3.60 g/cc
0.0939 - 0.130 lb/in³
Alliance BIF-2 Bonded (Composite) Magnetic Material
Density 2.60 - 3.60 g/cc
0.0939 - 0.130 lb/in³
Alliance BIF-16 Bonded (Composite) Magnetic Material