Polymer Property : Density = 0.1267 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 3.507 g/cc
0.1267 lb/in³
Laminate Density
Hardwire 3SX-21.5-12 High Density Composite
The 3SX Hardwire is a high carbon steel cord with a micro-fine brass or AO-brass (Adhesion Optimized) coating. The 3SX cord is used where balanced compressive and tensile strengths are required as w..