Physical Properties Metric English Comments
Density 0.0990 - 0.126 g/cc
0.00358 - 0.00455 lb/in³
typical range; ISO 845
3A Composites Core Materials AIREX® R82.110 High Performance Structural Foam
AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines outstanding fire resistance with low smoke and toxicity, along with excellent dielectric properties. It has a good strength to ..