Physical Properties Metric English Comments
Density 3.15 - 3.25 g/cc
0.114 - 0.117 lb/in³
molded; ASTM D792
Guarniflon PTFE G427 Polytetrafluoroethylene 40% Bronze, 5% Molybdenum Disulfide
PTFE G Special Compound with bronze and molybdenum disulphiteInformation provided by Guarniflon®