Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.93 g/cc | 0.106 lb/in³ | |
Pyrotek Pyrocast ZI Refractory Shapes Aggregate Base: BauxiteApplicationsCrucible bottoms Information provided by Pyrotek. |
|||
Density | 2.93 g/cc | 0.106 lb/in³ | calculated from bulk density after subtracting pore volume |
MarkeTech Repton EXP 93 Cordierite Mullite REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa.. |
|||
Density | 2.93 g/cc | 0.106 lb/in³ | |
LATI Latigray 82-02 CX/80 PA 12 Radiopaque compound based on Polyamide 12 (PA12). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Density | 2.94 g/cc | 0.106 lb/in³ | |
Schott LLF1 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 2.94 g/cc | 0.106 lb/in³ | |
Schott RG830 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6.. |
|||
Density | 2.93 g/cc | 0.106 lb/in³ | |
Schott RG850 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6.. |
|||
Density | 2.94 g/cc | 0.106 lb/in³ | |
BASF Heligoen® Green L 9361 Color Additive Description: Phthalocyanine green with extremely yellow and brilliant shadeChemical Structure: Cu Cu-phthalocyanine, brominatedPhysical form: PowderSuitable for: Baking systems, Waterborn systems, A.. |