Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.787 g/cc | 0.1007 lb/in³ | |
Pyrotek Valcor® G Pre-Cast Shapes ApplicationsBurner blocks Skimmer blocks Cover blocks Specialty blocks Plungers Stirrers Spouts Feeder tubes AdvantagesProven performance in molten glass contact applications Smooth surface finish d.. |