Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.780 - 2.77 g/cc | 0.0282 - 0.100 lb/in³ | Average value: 0.952 g/cc Grade Count:729 |
Overview of materials for Polypropylene Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp.. |