Physical Properties Metric English Comments
Density 2.63 g/cc

@Temperature 25.0 °C
0.0950 lb/in³

@Temperature 77.0 °F
Schott Glass 8252 Alkaline Earth Aluminosilicate Glass
Alkaline earth aluminosilicate glass for high temperature applications in electrical engineering, for sealing to molybdenum, free from alkali Bulb and exhaust tube for halogen lamps for automotive,..