Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.0929 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.0929 g/cc
0.00336 lb/in³
Core
Lendell Nolatex® Latex Free Foam
This foam is used in the cosmetics industry and also possesses insulation qualities.Applications:Cosmetic Wedges and Puffs, Padding, High Insulative Value Applications, Makovers ® Disposable Make..