Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.57 g/cc | 0.0928 lb/in³ | |
Mykroy/Mycalex MM 601 Molding Grade Glass-bonded Mica Composite Synthetic/Natural Mica Filler. Does not burn. ROHS Compliant.This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting demands of technical markets,.. |
|||
Density | 2.57 g/cc | 0.0928 lb/in³ | |
Specialty Materials Boron Monofilament Exceptional compression strength. Specialty Materials' Chemical Vapor Deposition process uses fine tungsten wire for the substrate and boron trichloride gas as the boron source.Information prov.. |
|||
Density | 2.57 g/cc | 0.0928 lb/in³ | |
Schott BG23 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |