Polymer Property : Density = 0.08999 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 2.491 g/cc
0.08999 lb/in³
Pyrotek MCX-40 Insulating Board
MCX-40 is a bonded-mica composite for use in glass contact applications. Its high operating temperature, low porosity, and low thermal conductivity make it ideal for all areas of hot glass transfer..