Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.40 g/cc | 0.0866 lb/in³ | Laminate Density |
Hardwire 3SX-12-12 Medium Density Composite The 3SX Hardwire is a high carbon steel cord with a micro-fine brass or AO-brass (Adhesion Optimized) coating. The 3SX cord is used where balanced compressive and tensile strengths are required as w.. |