Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.39 g/cc | 0.0862 lb/in³ | |
BNZ Materials Blazecrete 3200 Dense Castable Blazecrete 3200 is a high alumina castable for service to 3200°F (1778°C). It has good volume stability, extremely high modulus of rupture and crushing strength, and is of high purity for special .. |