Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.350 g/cc | 0.08490 lb/in³ | |
Reade Advanced Materials Montmorillonite - Smectite ((Na,Ca)(Al,Mg)6(Si4O10)3(OH)6-nH2O) Description: A clay mineral having a 2:1 expanding crystal lattice. Isomorphous substitution gives the various types and causes a net permanent charge balanced by cations in such a manner that water.. |
|||
Density | 2.350 - 2.470 g/cc | 0.08490 - 0.08924 lb/in³ | |
Reade Advanced Materials Petalite Powder (Li2O·Al2O3·8SiO2) Description: Rare, light and fragile with tabular or columnar crystals. A monoclinic mineral with a framework silicate structure. Its color is creamy to white and sometimes to more rarely pinkish. I.. |