Polymer Property : Density = 0.0845 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 2.34 g/cc
0.0845 lb/in³
Green Density
Nabaltec NABALOX® NO 315 Ground Alumina
NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula..
Density 2.34 g/cc
0.0845 lb/in³
Premix Thermoplastics PRESEAL® TPE 5010
PRESEAL TPE 5010 is a thermoplastic elastomer based highly conductive compound intended primarily for EMI gasket applications. It may also find interesting uses as conductors or in grounding applica..
Density 2.34 g/cc
0.0845 lb/in³
Pyrotek Pyrocast ZR Refractory Shapes
Aggregate Base: Fused Silica / MulliteApplicationsTransfer troughs Information provided by Pyrotek.
Density 2.34 g/cc
0.0845 lb/in³
Schott NG12 Neutral Density Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include NG3, NG4, NG5, NG9, NG10, NG11, NG 1
Density 2.34 g/cc

@Temperature 25.0 °C
0.0845 lb/in³

@Temperature 77.0 °F
Schott FIOLAX® clear Neutral Glass Tubing
Neutral glass tubing, chemically highly resistant Pharmaceutical primary packagingInformation provided by SCHOTT AG.
Density 2.34 g/cc

@Temperature 25.0 °C
0.0845 lb/in³

@Temperature 77.0 °F
Schott DUROBAX® clear Neutral Glass Tubing
Neutral glass tubing, chemically highly resistant Syringes, cartridges, chemical and technical apparatus The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is..