Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.0949 g/cc | 0.075677 lb/in³ | |
Saint-Gobain Chemfab® 6 High-Performance PTFE-Coated Glass Description: Chemfab® High-Performance Series provides the highest level of PTFE content for superior surface smoothness, durability, and longer life. Use this product for the most demanding heat.. |