Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.0470 g/cc | 0.073946 lb/in³ | |
Saint-Gobain Chemfab® 6 Premium PTFE-Coated Glass Description: Chemfab® Premium Series combines a superior quality glass fabric with a high level of PTFE content. Description: Chemfab® Premium is an excellent multi-purpose fabric with a smoot.. |