Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0737 g/cc | 0.00266 lb/in³ | Nominal Core Density |
Unifrax Fiberfrax® Lo-Con™ Felt Fiberfrax® Lo-Con™ felt and Duraset® flet are unique product forms in the Unifrax Corporation's extensive ceramic fiber product family. Felt products extend the performance of Fiberfrax papers i.. |