Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.0293 g/cc | 0.073304 lb/in³ | |
Saint-Gobain Chemfab® 10 Tear Resistant PTFE-Coated Glass Description: Chemfab® Tear Resistant Series is manufactured with specialized coating materials to improve tear and crease resistance. Uses for this series includes release sheets, belting and gas.. |
|||
Density | 2.0293 g/cc | 0.073304 lb/in³ | |
Saint-Gobain Chemfab® 5 Premium PTFE-Coated Glass Description: Chemfab® Premium Series combines a superior quality glass fabric with a high level of PTFE content. Description: Chemfab® Premium is an excellent multi-purpose fabric with a smooth, h.. |