Polymer Property : Density = 0.07110 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.968 g/cc
0.07110 lb/in³
ASTM D1505
DuPont Elvax® 40L-08 Ethylene-Vinyl Acetate Copolymer Resin  (discontinued **)
Elvax® 40L-08 is an ethylene-vinyl acetate copolymer that is useful in many wire and cable applications because of its excellent mechanical, thermal, and low-smoke properties. The melt index is ap..