Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0500 - 0.0700 g/cc | 0.00181 - 0.00253 lb/in³ | ISO 845-88 |
Eurofoam Porocell POR 300/60 Ethylene Octane Metallocene EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Density | 0.0600 - 0.0700 g/cc | 0.00217 - 0.00253 lb/in³ | typical range; ISO 845 |
3A Composites Core Materials AIREX® T90.60 Easy Processing Structural FST Foam AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu.. |