Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.802 - 1.936 g/cc | 0.06510 - 0.06992 lb/in³ | |
Saint-Gobain Chemfab® SlipGrip™ 6 PTFE/Silicone Coated Fiberglass Fabric Description: SlipGrip™ products are PTFE-coated fiberglass fabrics with silicone rubber on one face. This unique combination provides a "slippery" PTFE surface and a "grippy" silicone surface. .. |