Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.584 g/cc | 0.05723 lb/in³ | ISO 1183 |
Stir SpA IN 3000 G IG (PVC) Application: Extrusion fillerInformation provided by STIR SpA |
|||
Density | 1.584 g/cc | 0.05723 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP JF006 PES LNP* THERMOCOMP* JF006 is a compound based on Polyethersulfone resin containing 30% Glass Fiber. |