Density 0.0560 g/cc
0.00202 lb/in³
core density
Ultracor® UCF-355-3/8-3.5 Honeycomb Core Material
Construction: ±45° T300. Fiber: Carbon T300. Ultracor® is a very low density honeycomb core material designed for use in highly weight-sensitive structures.  It is expected that it will be use..
Density 0.0560 g/cc
0.00202 lb/in³
Molded density, ASTM D1622
Covestro Bayfill® EA 4002 Polyurethane Energy-Absorbing Semi-Rigid Foam, Rigid Grade, MDI-based 2-Component Liquid System
Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.