Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.538 g/cc | 0.05556 lb/in³ | |
Pyrotek F-10 Silicone Core Rope Silicone core with double jacket of heavy gauge fiberglass cloth. Silicone coated overall.AdvantagesGood Abrasion Resistance Good Compression and Recall Information provided by Pyrotek. |
|||
Density | 1.538 g/cc | 0.05556 lb/in³ | ISO 1183 |
Stir SpA HE 62 1 (PVC) Application: Extrusion rolling shutters - various profilesInformation provided by STIR SpA |
|||
Density | 1.538 g/cc | 0.05556 lb/in³ | |
3M Novec™ 7100 Engineered Fluid 3M™ Novec™ 7100 Engineered Fluid, methoxy-nonafluorobutane (C4F9OCH3), is a clear, color less and low-odor fluid intended to replace ozone-depleting substances (ODSs) and compounds with high globa.. |