Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.49 g/cc | 0.0540 lb/in³ | ASTM D792 |
Ensinger DELRIN® 100AF Acetal Homopolymer, 13% PTFE filled (POM) Ensinger’s DELRIN®100AF blend stock shapes are a 13% PTFE fiber filled homopolymer acetal. They offer an improved coefficient of friction, better lubricity, and improved wear characteristics over .. |
|||
Density | 1.49 g/cc | 0.0540 lb/in³ | ASTM D792 |
Ensinger DELRIN® 570 Acetal, 20% Glass Filled (POM) DELRIN®570 Shapes manufactured by Ensinger are 20% glass filled materials intended for general industrial use. The material offers very high stiffness, low warpage, and low creep for superior part .. |