Physical Properties Metric English Comments
Density 1.387 g/cc
0.05011 lb/in³
ASTM D 792
SABIC Innovative Plastics LNP Stat-kon EX08308C PEI (Asia Pacific)
Stat-Kon* EX08308C is a high cleanliness Polyetherimide Compound reinforced with Carbon Fiber for use in applications requiring the highest level of cleanliness. This compound is compounded using LN..