Density 1.324 g/cc
0.04783 lb/in³
ISO 1183
Lanxess Durethan® DP AKV 30 X HR EF 900116 Nylon 66, 30% Glass Fiber
PA 66, injection molding grade, 30% glass fibers, hydrolysis and good heat-ageing resistance, good flowability (Easy Flow)
Density 1.324 g/cc
0.04783 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP UC006H PPA
LNP THERMOCOMP* UC006H is a compound based on Polyphthalamide resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare.