Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.313 g/cc | 0.04744 lb/in³ | |
Pyrotek TS-82 Thermoset Electrical Insulation Product (Nema Grade: XXX) Paper reinforcement, Phenolic Resin, Natural Color. High humidity resistance, Excellent resistance to splitting.Information provided by Pyrotek. |
|||
Density | 1.313 g/cc | 0.04744 lb/in³ | JIS-Z-8807 |
Denka VINYKON W7100i PVC, W grade for non-migratory sheath and special items A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |