Density 1.305 g/cc
0.04715 lb/in³
ISO 1183
Stir SpA B 3060 AT (PVC)
Application: Molding for boot-legInformation provided by STIR SpA
Density 1.305 g/cc
0.04715 lb/in³
JIS-Z-8807
Denka VINYKON W7300E PVC, W grade for non-migratory sheath and special items
A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding..