Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.302 g/cc | 0.04704 lb/in³ | ISO 1183 |
Lanxess Durethan® BKV 230 DUS008 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fiber, injection molding, impact modified, heat-ageing stabilizedInformation provided by LANXESS. |
|||
Density | 1.302 g/cc | 0.04704 lb/in³ | ISO 1183 |
Stir SpA SR 94 T (PVC) Application: Primarily for telephoneInformation provided by STIR SpA |
|||
Density | 1.302 g/cc | 0.04704 lb/in³ | JIS-Z-8807 |
Denka VINYKON M2510 PVC, M grade for soft injection molding A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |