Polymer Property : Density = 0.0460 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.0380 - 0.0460 g/cc
0.00137 - 0.00166 lb/in³
Akzo Nobel Expancel® 551 DE 40 d42 Dry expanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Density 0.0380 - 0.0460 g/cc
0.00137 - 0.00166 lb/in³
Akzo Nobel Expancel® 551 DE 80 d42 Dry expanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..