Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.273 g/cc | 0.04599 lb/in³ | ASTM D3165 |
Vicone High Performance Rubber VicoSil™ C306E-GR High Performance Silicone Rubber Information provided by Vicone |
|||
Density | 1.273 g/cc | 0.04599 lb/in³ | JIS-Z-8807 |
Denka VINYKON G5070 PVC, W grade for non-migratory sheath and special items A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |