Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.27 g/cc | 0.0457 lb/in³ | Fired Density at 2000°F |
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M100 Moldable Description: A family of high temperature moldables designed for a wide variety of uses. THERMOSEAL® FIBERPAK® MOLDABLES may be formed into shapes or linings, pushed into cracks and holes, or .. |