Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.25 g/cc | 0.0450 lb/in³ | Yield Density |
Honeywell Capran® Emblem™ 1530 PVDC-Coated Bi-Axially Oriented Nylon Film
(discontinued **) Capran® Emblem™ 1530 is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbons, and many .. |
|||
Density | 1.25 g/cc | 0.0450 lb/in³ | ASTM D792 |
Ensinger TECASON™ S Polysulfone (PSU) TECASON™ S is a transparent engineering plastic known for its chemical resistance, rigidity, high-temperature performance, and its ability to operate in an autoclave environment. TECASON™ S is FD.. |