Physical Properties Metric English Comments
Density 1.245 g/cc
0.04498 lb/in³
ASTM D792
SABIC Innovative Plastics Lexan® 500 PC
10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance.
Density 1.245 g/cc
0.04498 lb/in³
ASTM D792
SABIC Innovative Plastics Lexan® 500 PC (Asia Pacific)
10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance.
Density 1.245 g/cc
0.04498 lb/in³
ASTM D792
SABIC Innovative Plastics Lexan® 500R PC
10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. Internal mold release.
Density 1.245 g/cc
0.04498 lb/in³
ASTM D792
SABIC Innovative Plastics Lexan® 500R PC (Asia Pacific)
10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. Internal mold release.
Density 1.245 g/cc
0.04498 lb/in³
ASTM D792
SABIC Innovative Plastics Lexan® 503 PC
10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized.
Density 1.245 g/cc
0.04498 lb/in³
ASTM D792
SABIC Innovative Plastics Lexan® 503 PC (Asia Pacific)
10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized.
Density 1.245 g/cc
0.04498 lb/in³
ASTM D792
SABIC Innovative Plastics Lexan® 503R PC
10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. Internal mold release.
Density 1.245 g/cc
0.04498 lb/in³
ASTM D792
SABIC Innovative Plastics Lexan® 503R PC (Asia Pacific)
10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. Internal mold release.
Density 1.245 g/cc

@Temperature 25.0 °C
0.04498 lb/in³

@Temperature 77.0 °F
Shandong Dongyue Polymer HFC-125 Pentafluoroethane Refrigerant, CHF2CF3
Usage: Component of mixture used as refrigerant substituting for CFC-502 and HCFC-22; Fire extinguishing agent substituting for Halon-1211 and Halon-1301Packing: Transport by cylinder or tank, the l..
Density 1.245 g/cc
0.04498 lb/in³
ISO 1183
Stir SpA C 2036 DS AT (PVC)
Application: Molding for solesInformation provided by STIR SpA
Density 1.245 g/cc
0.04498 lb/in³
ISO 1183
Stir SpA CT 80 ATC R (PVC)
Application: Tread, pure plasticInformation provided by STIR SpA
Density 1.245 g/cc
0.04498 lb/in³
ASTM D792
SABIC Innovative Plastics NORYL GTX GTX820 PPE+PS+PA
GR 20%. Higher stiffness of 800000 psi (4000 MPa) flexural modulus. Excellent chemical and high heat resistance. Application: valves.
Density 1.245 g/cc
0.04498 lb/in³
ASTM D792
SABIC Innovative Plastics NORYL GTX GTX820 PPE+PS+PA (Asia Pacific)
GR 20%. Higher stiffness of 800000 psi (4000 MPa) flexural modulus. Excellent chemical and high heat resistance. Application: valves.
Copyright © lookpolymers.com All Rights Reserved