Polymer Property : Density = 0.0442 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.17 - 1.22 g/cc
0.0424 - 0.0442 lb/in³
Lord Adhesives 202 Semi-Flexible, Fast Cure, Medium Viscosity Acrylic Adhesive
Lord 200 SeriesLord 200 Series Acrylic Adhesives bond minimally prepared or unprepared surfaces. They offer excellent adhesion to unprepared metals, ceramic magnets and plastics. Viscosities range f..