Physical Properties Metric English Comments
Density 1.192 g/cc
0.04306 lb/in³
LATI Latiohm 90/13-09 PD01 G/10 PPOm, 10% Glass Fiber Reinforced
Semiconductive/dissipative product based on Modified Polyphenylene Oxide (PPOm). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation prov..