Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.155 - 1.175 g/cc | 0.04173 - 0.04245 lb/in³ | L140 |
Solvay CATAFOR® MS/T Surfactant Description: Proprietary blendIdentification: ALKALI METAL SALT IN SOLVENTSoluble in polar organic solvent. Soluble in water.pH: NeutralAvailable in: Asia Pacific, Europe, Latin America and North Am.. |