Physical Properties Metric English Comments
Density 1.138 g/cc
0.04111 lb/in³
method A; ISO 1183:1987
Nylacast Oilon Cast Nylon 6, Lubricated (Lubricant Oil Filled)
This exceptional oil-loaded nylon features a complex blended oil lubrication system, uniformly distributed throughout the product, that guarantees constant performance over the whole service life. E..